| 1. | Therefore, nanoindentation test is used to determine the elastic modulus of these materials.
|
| 2. | Nanoindentation measurements have reported hardness as great as 50 % more than values for natural crystalline diamond.
|
| 3. | Many mechanical and imaging techniques such as nanoindentation and atomic force microscopy are used to characterize these tissues.
|
| 4. | A "'nanoindenter "'is the main component for indentation hardness tests used in nanoindentation.
|
| 5. | Since the mid-1970s nanoindentation has become the primary method for measuring and testing very small volumes of mechanical properties.
|
| 6. | Hardness of 6 GPa and a modulus of 210 GPa were measured by nanoindentation and hollow tube compression experiments, respectively ..
|
| 7. | In nanoindentation small loads and tip sizes are used, so the indentation area may only be a few square micrometres or even nanometres.
|
| 8. | The ability to conduct nanoindentation studies with nanometer depth, and sub-nanonewton force resolution is also possible using a standard AFM setup.
|
| 9. | The nanoindentation values were found to be 36.4 GPa and 34.0 GPa for the ( 002 ) and perpendicular planes respectively.
|
| 10. | As it is three sided, it is easier to grind these tips to a sharp point and so is more readily employed for nanoindentation tests.
|